Olympus-OM
[Top] [All Lists]

Re: [OM] OT - Dessicants

Subject: Re: [OM] OT - Dessicants
From: Garth Wood <garth@xxxxxxxxxxxxxxx>
Date: Thu, 05 Aug 1999 20:35:03 -0600
At 12:17 AM 8/6/99 +0000, Giles wrote:
>
>These plastic capsules are what I use, they recharge fine in an oven.  I set 
>mine to 
>40-50 C.

Giles:

That's fine I guess, if you can actually set your oven that low...  (mine's a 
newer convection oven that won't set below 175 degrees Fahrenheit).  
Personally, I'd be afraid of the plastic canisters melting in the oven.  At 300 
degrees Fahrenheit, 50 grams of silica gel dessicant takes about three hours to 
completely re-activate.

Garth